Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 14.0 MPa @Strain 1 % |
2030 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Semitron® ESd 225 POM-C, static dissipative, extruded (ISO Data) Semitron ESd 225 is an acetal based static dissipative material ideal for material handling operations. It is also an excellent choice for fixturing used in the manufacturing of hard disk drives or .. |
|||
Compressive Strength | 14.0 - 18.0 MPa @Temperature 100 °C |
2030 - 2610 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |