Polymer Property : Compressive Strength = 18.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 18.6 MPa

@Temperature 1095 °C
2700 psi

@Temperature 2003 °F
Cold Crush Strength
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..
Compressive Strength 18.6 MPa

@Temperature 1095 °C
2700 psi

@Temperature 2003 °F
Cold Crush Strength
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..