Mechanical Properties Metric English Comments
Compressive Strength 18.0 MPa

@Strain 5 %
2610 psi

@Strain 5 %
ISO 604
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
Compressive Strength 18.0 MPa

@Strain 5 %
2610 psi

@Strain 5 %
ISO 604
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne..