Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 150 - 170 MPa @Temperature 1300 °C |
21800 - 24700 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Compressive Strength | 150 - 170 MPa @Temperature 1600 °C |
21800 - 24700 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |