Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0981 MPa @Temperature 1000 °C |
14.2 psi @Temperature 1830 °F |
Cold Crushing |
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |