Polymer Property : Compressive Strength = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 90.0 MPa

@Strain 5 %
13100 psi

@Strain 5 %
ISO 604
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data)
This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear..
Compressive Strength 90.0 MPa

@Temperature 200 °C
13100 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Compressive Strength 90.0 MPa

@Temperature 200 °C
13100 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Compressive Strength 90.0 MPa

@Temperature 120 °C
13100 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Compressive Strength 90.0 MPa

@Temperature 120 °C
13100 psi

@Temperature 248 °F
ISO 604
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Compressive Strength 90.0 - 110 MPa

@Temperature 1600 °C
13100 - 16000 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material
Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can..
Compressive Strength 90.0 - 110 MPa

@Temperature 1300 °C
13100 - 16000 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 90.0 - 110 MPa

@Temperature 1300 °C
13100 - 16000 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app..
Compressive Strength 90.0 - 110 MPa

@Temperature 1300 °C
13100 - 16000 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable
Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Compressive Strength 90.0 - 110 MPa

@Temperature 100 °C
13100 - 16000 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable
Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib..
Compressive Strength 90.0 - 110 MPa

@Temperature 1400 °C
13100 - 16000 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable
Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista..
Compressive Strength 90.0 - 110 MPa

@Temperature 1400 °C
13100 - 16000 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable
Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl..
Compressive Strength 90.0 - 110 MPa

@Temperature 1300 °C
13100 - 16000 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Compressive Strength 90.0 - 110 MPa

@Temperature 1600 °C
13100 - 16000 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable
Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In..
Compressive Strength 90.0 - 110 MPa

@Temperature 1500 °C
13100 - 16000 psi

@Temperature 2730 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable
Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont..
Compressive Strength 90.0 MPa

@Temperature 110 °C
13100 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics VELECRETE RC 103 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Compressive Strength 90.0 MPa

@Temperature 1400 °C
13100 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics VELECRETE RC 103 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Compressive Strength 90.0 MPa

@Temperature 1000 °C
13100 psi

@Temperature 1830 °F
Cold Crushing
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Compressive Strength 90.2 MPa

@Temperature 1000 °C,
Time 10800 sec
13100 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 90.2 MPa

@Temperature 110 °C,
Time 86400 sec
13100 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 90.0 MPa

@Temperature 120 °C
13100 psi

@Temperature 248 °F
Result based on HT G22; ISO 604
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..
Compressive Strength 90.0 - 110 MPa

@Temperature 1000 °C
13100 - 16000 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable
Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t..