Polymer Property : Compressive Strength = 125 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 115 - 125 MPa

@Temperature 100 °C
16700 - 18100 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material
Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed ..