Polymer Property : Compressive Strength = 114000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 786 MPa

@Temperature 21.1 °C
114000 psi

@Temperature 70.0 °F
Dry; Vacuum/Oven Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Compressive Strength 786 MPa

@Temperature 21.1 °C
114000 psi

@Temperature 70.0 °F
Dry, 0° Direction; ASTM D695
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..