Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 69.0 MPa @Strain 1 % |
10000 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data) This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein.. |
|||
Compressive Strength | 69.0 MPa @Strain 5 % |
10000 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Compressive Strength | 69.0 MPa @Strain 2 % |
10000 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Compressive Strength | 68.9 MPa @Temperature 288 °C |
10000 psi @Temperature 550 °F |
ASTM D-695 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |