Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 6.89 MPa @Treatment Temp. 540 °C |
1000 psi @Treatment Temp. 1000 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |