Mechanical Properties Metric English Comments
Compressive Strength 10.8 MPa

@Temperature 110 °C,
Time 86400 sec
1560 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing, Typical Value, After drying @ 110°C
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic
Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 10.8 MPa

@Temperature 800 °C
1560 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 1.5 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 10.8 MPa

@Temperature 1000 °C,
Time 10800 sec
1560 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).