Polymer Property : Compressive Strength = 0.500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.300 - 0.500 MPa

@Temperature 815 °C
43.5 - 72.5 psi

@Temperature 1500 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..