Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.300 - 0.500 MPa @Temperature 815 °C |
43.5 - 72.5 psi @Temperature 1500 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning .. |