Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 64.8 GPa @Temperature 121 °C |
9400 ksi @Temperature 250 °F |
0° Direction, Dry, 365° Oven Cured; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Tensile Modulus | 64.8 GPa @Temperature 121 °C |
9400 ksi @Temperature 250 °F |
0° Direction, Wet, 365° Oven Cured; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Tensile Modulus | 64.8 GPa @Temperature 19.4 °C |
9400 ksi @Temperature 67.0 °F |
CTD, 90° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Tensile Modulus | 64.8 GPa @Temperature -55.0 °C |
9400 ksi @Temperature -67.0 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Tensile Modulus | 64.8 GPa @Temperature -59.0 °C |
9400 ksi @Temperature -74.2 °F |
T300, Plain Weave; Fill Tension; |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form Fiber: T300-3KInformation provided by HexCel |
|||
Tensile Modulus | 64.8 GPa @Temperature 200 °C |
9400 ksi @Temperature 392 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |