Mechanical Properties Metric English Comments
Tensile Modulus 9.58 GPa

@Temperature 77.0 °C
1390 ksi

@Temperature 171 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel