Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.60 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 8.60 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
|
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 8.60 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
|
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Tensile Modulus | 8.60 GPa @Temperature 150 °C |
1250 ksi @Temperature 302 °F |
|
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |