Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 8.41 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.41 GPa

@Temperature 200 °C
1220 ksi

@Temperature 392 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel