Mechanical Properties Metric English Comments
Tensile Modulus 6.41 GPa

@Temperature 121 °C
930 ksi

@Temperature 250 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..