Mechanical Properties Metric English Comments
Tensile Modulus 0.400 GPa

@Temperature 150 °C
58.0 ksi

@Temperature 302 °F
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Tensile Modulus 0.400 GPa

@Temperature 150 °C
58.0 ksi

@Temperature 302 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 0.400 GPa

@Temperature 23.0 °C
58.0 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
Tensile Modulus 0.400 GPa

@Temperature 80.0 °C
58.0 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8253 HS PA6 (Dry)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
Tensile Modulus 0.400 GPa

@Temperature 50.0 °C
58.0 ksi

@Temperature 122 °F
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Tensile Modulus 0.400 GPa

@Temperature 120 °C
58.0 ksi

@Temperature 248 °F
LATI Later 4 PBT
Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 0.400 GPa

@Temperature 100 °C
58.0 ksi

@Temperature 212 °F
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..