Tensile Modulus 0.330 GPa

@Temperature 90.0 °C
47.9 ksi

@Temperature 194 °F
LATI Latamid 66 E21 PA 66, Impact Modified
Polyamide 66 (PA66). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
Tensile Modulus 0.330 GPa

@Temperature 150 °C
47.9 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..