Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.17 GPa @Temperature 23.0 °C |
460 ksi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |