Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 27.3 GPa @Temperature -54.0 °C |
3960 ksi @Temperature -65.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |