Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.291 GPa @Temperature -40.0 °C |
477.3 ksi @Temperature -40.0 °F |
DAM; ISO 527 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |