Polymer Property : Tensile Modulus = 3.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Tensile Modulus 3.10 GPa

@Temperature 150 °C
450 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 3.10 GPa

@Temperature 150 °C
450 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
LATI Latamid 66 PA 66
Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 3.10 GPa

@Temperature 120 °C
450 ksi

@Temperature 248 °F
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 3.10 GPa

@Temperature 150 °C
450 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D..
Tensile Modulus 3.10 GPa

@Temperature 120 °C
450 ksi

@Temperature 248 °F
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer
Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..