Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 24.4 GPa @Temperature 177 °C |
3540 ksi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel |