Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.59 GPa @Temperature 23.9 °C |
375 ksi @Temperature 75.0 °F |
|
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |
|||
Tensile Modulus | 2.59 GPa @Thickness 4.00 mm, Temperature 30.0 °C |
376 ksi @Thickness 0.157 in, Temperature 86.0 °F |
|
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |