Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.0 GPa @Temperature 23.0 °C |
1890 ksi @Temperature 73.4 °F |
|
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Tensile Modulus | 13.0 GPa @Temperature 120 °C |
1890 ksi @Temperature 248 °F |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 13.0 GPa @Temperature 120 °C |
1890 ksi @Temperature 248 °F |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Tensile Modulus | 13.0 GPa @Temperature 60.0 °C |
1890 ksi @Temperature 140 °F |
|
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Tensile Modulus | >= 13.0 GPa @Temperature 200 °C |
>= 1890 ksi @Temperature 392 °F |
|
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |