Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.950 GPa @Temperature 90.0 °C |
138 ksi @Temperature 194 °F |
|
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif.. |
|||
Tensile Modulus | 0.950 GPa @Temperature 60.0 °C |
138 ksi @Temperature 140 °F |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |