Polymer Property : Tensile Modulus = 0.950 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.950 GPa

@Temperature 90.0 °C
138 ksi

@Temperature 194 °F
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif..
Tensile Modulus 0.950 GPa

@Temperature 60.0 °C
138 ksi

@Temperature 140 °F
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..