Polymer Property : Tensile Modulus = 1350 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.30 GPa

@Temperature 150 °C
1350 ksi

@Temperature 302 °F
ISO 527
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..
Tensile Modulus 9.30 GPa

@Temperature 90.0 °C
1350 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 9.30 GPa

@Temperature 23.0 °C
1350 ksi

@Temperature 73.4 °F
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Tensile Modulus 9.30 GPa

@Temperature 23.0 °C
1350 ksi

@Temperature 73.4 °F
LATI Latamid SP2 H2 G/35 PA 6.12, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 9.30 GPa

@Temperature 90.0 °C
1350 ksi

@Temperature 194 °F
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti..
Tensile Modulus 9.30 GPa

@Temperature 23.0 °C
1350 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..