Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.700 GPa

@Temperature 150 °C
102 ksi

@Temperature 302 °F
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 0.700 GPa

@Temperature 120 °C
102 ksi

@Temperature 248 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 0.700 GPa

@Temperature 90.0 °C
102 ksi

@Temperature 194 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 0.700 GPa

@Temperature 60.0 °C
102 ksi

@Temperature 140 °F
LATI Latamid SP1 PA 6.10
Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..
Tensile Modulus 0.700 GPa

@Temperature 260 °C
102 ksi

@Temperature 500 °F
ASTM D 638
Saint-Gobain Meldin® 2211 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser..
Tensile Modulus 0.700 GPa

@Temperature 120 °C
102 ksi

@Temperature 248 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Tensile Modulus 0.700 GPa

@Temperature 50.0 °C
102 ksi

@Temperature 122 °F
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..