Polymer Property : Tensile Modulus = 1.259 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.259 GPa

@Temperature 40.0 °C
182.6 ksi

@Temperature 104 °F
DAM; ISO 527
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers