Mechanical Properties Metric English Comments
Tensile Modulus 0.320 GPa

@Temperature 90.0 °C
46.4 ksi

@Temperature 194 °F
LATI Latamid 6 E02 PA 6, Impact modified
Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A...