Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.150 GPa @Temperature 150 °C |
21.8 ksi @Temperature 302 °F |
|
LATI Latamid 6 E02 PA 6, Impact modified Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A... |