Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 860 MPa @Diameter 12.7 mm |
125000 psi @Diameter 0.500 in |
As Welded |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 860 MPa @Temperature 425 °C |
125000 psi @Temperature 797 °F |
Precipitation Hardened prior to test |
Special Metals MONEL® Alloy K-500 A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under.. |