Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 80.0 MPa @Temperature -40.0 °C |
11600 psi @Temperature -40.0 °F |
ASTM D638 |
BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Tensile Strength, Ultimate | 80.0 MPa @Temperature -40.0 °C |
11600 psi @Temperature -40.0 °F |
ISO 527 |
BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Tensile Strength, Ultimate | 80.0 MPa @Temperature 80.0 °C |
11600 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 80.0 MPa @Temperature -40.0 °C |
11600 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |