Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 778 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
113000 psi

@Thickness 0.500 in,
Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Ultimate 778 MPa

@Thickness 3.20 mm,
Temperature 427 °C
113000 psi

@Thickness 0.126 in,
Temperature 801 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Ultimate 778 MPa

@Thickness 19.1 mm,
Temperature 93.0 °C
113000 psi

@Thickness 0.752 in,
Temperature 199 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..