Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4890 MPa

@Temperature 23.0 °C
709000 psi

@Temperature 73.4 °F
AGY ZenTron® S-2 Generic S-Glass Fiber
S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod..