Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.0%); ASTM-D638 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |