Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 276 MPa @Temperature 427 °C |
40000 psi @Temperature 800 °F |
SAE 1020 Steel butt joint |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Tensile Strength, Ultimate | 276 MPa @Temperature 649 °C |
40000 psi @Temperature 1200 °F |
Type 304 Stainless Steel butt joint |
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy Applications:Premabraze 130 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |
|||
Tensile Strength, Ultimate | 276 MPa @Temperature 649 °C |
40000 psi @Temperature 1200 °F |
Type 304 Stainless Steel butt joint |
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy Applications:Premabraze 131 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |