Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 195 MPa @Temperature 23.0 °C |
28300 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 195 MPa @Temperature -40.0 °C |
28300 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.4%); ASTM-D638 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 195 MPa @Temperature 10.0 °C |
28300 psi @Temperature 50.0 °F |
|
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur.. |