Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.0 MPa

@Temperature 100 °C
2610 psi

@Temperature 212 °F
Y direction, Condition A; ASTM D638
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..