Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 215 MPa @Temperature -40.0 °C |
31200 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 215 MPa @Temperature -40.0 °C |
31200 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.75%); ASTM-D638 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 215 MPa @Temperature 23.0 °C |
31200 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 215 MPa @Temperature 650 °C |
31200 psi @Temperature 1200 °F |
|
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained.. |