Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 134 MPa @Temperature 23.0 °C |
19400 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.4%); ASTM-D638 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |