Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa

@Temperature 427 °C
21000 psi

@Temperature 800 °F
SAE 1020 Steel sleeve joint
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi..
Tensile Strength, Ultimate 145 MPa

@Temperature -40.0 °C
21000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 145 MPa

@Temperature -40.0 °C
21000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.1%); ASTM-D638
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.75%); ASTM-D638
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 145 MPa

@Temperature 80.0 °C
21000 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
Practical Use; ASTM-D638
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 145 - 185 MPa

@Thickness 0.200 - 1.50 mm
21000 - 26800 psi

@Thickness 0.00787 - 0.0591 in
Aleris 55HX® Aluminum (5005-H14)
Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ..
Tensile Strength, Ultimate 145 - 185 MPa

@Thickness 1.50 - 3.00 mm
21000 - 26800 psi

@Thickness 0.0591 - 0.118 in
Aleris 55HX® Aluminum (5005-H14)
Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ..
Tensile Strength, Ultimate 145 - 185 MPa

@Thickness 3.00 - 5.00 mm
21000 - 26800 psi

@Thickness 0.118 - 0.197 in
Aleris 55HX® Aluminum (5005-H14)
Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ..