Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1010 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1010 MPa

@Temperature 20.0 °C
146000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
EDRO #2 Prehardened 4130 Holder Block
EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to i..
Tensile Strength, Ultimate 1010 MPa

@Temperature 20.0 °C
146000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..