Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.40 - 1.58 kN/m | 8.00 - 9.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |