Mechanical Properties Metric English Comments
Peel Strength 1.2161 kN/m
6.9375 pli
Stainless Steel, 90°, 72 hr at 70°C, Faceside; ASTM D3330
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and..