Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.2161 kN/m | 6.9375 pli | Stainless Steel, 90°, 72 hr at 70°C, Faceside; ASTM D3330 |
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and.. |