Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.50 kN/m @Temperature 22.2 °C |
31.4 pli @Temperature 72.0 °F |
Bell Peel |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.05 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |